41. Broken yarn in surface; non-friction side  
Broken yarn in surface; non-friction side Acceptable if: <=1% of area; <=30% of thickness, no more than 2 allowed.  
42. Broken yarn in surface; friction side  
Broken yarn in surface; friction side Acceptable if: <= 0,5% of area: <= 30% of thickness no more than 2 allowed.  
43. Blisters  
Blisters Not acceptable.  
44. Pressed in yarn  
"Pressed in" yarn Acceptable providing it is securely bonded to the disc and is wholly contained in one segment, no more than 2 allowed.  
45. Surface sealing faults  
Surface sealing faults Acceptable.  
46. Surface grind marks  
Surface grind marks Acceptable as long as dimensional specifications are maintained.  
47. Surface cracks  
Surface cracks Acceptable up to 25% of lining width up to 0,2 mm deep. Not acceptable across full lining width independent of depth.  
48. Surface blisters  
Surface blisters Not acceptable.  
49. Poor consolidation  
Poor consolidation Not acceptable.  
50. Plastic reinforcement in rivet hole (Sketch)  
Plastic reinforcement in rivet hole (Sketch) Acceptable.  