Skip to main content

VRI Webseitensuche

636 results:
51. Pitted surface (plucked surface)  
Pitted surface (plucked surface) Typical for certain materials. Acceptable.  
52. Paint on surface - Linings for riveting and bonding  
Paint on surface - Linings for riveting and bonding Acceptable up to 5% of area on both inside and outside surfaces, paint '"runs" not acceptable.  
53. Outside surface indentations - Commercial linings  
Outside surface indentations - Commercial linings Acceptable up to 30mm² - 1mm deep, no more than 2 allowed.  
54. Outside surface indentations - Car linings  
Outside surface indentations - Car linings Acceptable up to 20mm² - 1mm deep no more than 2 allowed.  
55. Moulding skin on outside radius surface - Linings for riveting or bonding  
Moulding skin on outside radius surface - Linings for riveting or bonding Acceptable up to 3% of surface area provided dimensional specifications are maintained.  
56. Moulding skin on inside radius surface - Linings for riveting  
Moulding skin on inside radius surface - Linings for riveting Where inside ground finish is specified up to 10% of surface acceptable, provided dimensional specifications are maintained.  
57. Moulding skin on inside radius suface - Linings for bonding  
Moulding skin on inside radius suface - Linings for bonding Where inside ground finish is specified up to 3% of surface acceptable provided the unground area is not at the lining ends and dimensional…  
58. Metal wire reinforcement showing in rivet hole (Sketch)  
Metal wire reinforcement showing in rivet hole (Sketch) Not acceptable.  
59. Metal wire reinforcement showing in rivet hole  
Metal wire reinforcement showing in rivet hole Not acceptable.  
60. Paint | Paint on friction material surface  
Paint on friction material surface Component Paint Characteristic Paint on friction material surface and chamfer Brake pads friction area ≤ 120 cm2 Acceptable up to 10% on contact surface…  
Search results 51 until 60 of 636